Polymer Property : 300% Modulus = 0.996 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00686 GPa
0.996 ksi
Cured
KKPC KOSYN KBR 01L Polybutadiene Rubber (High cis BR)
Polybutadiene Rubber (High cis BR)Characteristics: Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solut..
300% Modulus 0.00686 GPa
0.996 ksi
Taiwan Sheen Soon Sheenthane® A8631N Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.