Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00601 GPa | 0.872 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |