Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00501 GPa | 0.727 ksi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT.. |