Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00240 GPa | 0.348 ksi | ASTM D412 |
Kraton® G2806 GO-N (SEBS) Compound Description: Kraton G2806 GO-N is a compound designed for film applications in the Personal Care market: Kraton G2806 GO-N - supplied as an organic dusted dense pelletRegion: Asia Pacific, Europe, J.. |
|||
300% Modulus | 0.00240 GPa | 0.348 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |