Mechanical Properties Metric English Comments
300% Modulus 0.00152 GPa
0.220 ksi
ASTM D 412
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
300% Modulus 0.00152 GPa
0.220 ksi
ASTM D 412
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
300% Modulus 0.00152 GPa
0.220 ksi
ASTM D 412
CPT C-Flex® R70-081 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..