Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000689 GPa | 0.100 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2720 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.000689 GPa | 0.100 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.000689 GPa | 0.100 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |