Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000683 GPa @Time 7200 sec |
0.0990 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7345-1000 TPE Product Description: StarFlex P 7345-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
300% Modulus | 0.000683 GPa @Time 7200 sec |
0.0990 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |