Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000655 GPa @Time 7200 sec |
0.0950 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-9000 TPE Product Description: StarGrip GP 25-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubber.. |