Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000500 GPa | 0.0725 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 9133 Styrene - Isoprene Block Copolymer Europrene® SOL T 9133 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 16% weight and diblock content is.. |
|||
300% Modulus | 0.000500 GPa | 0.0725 ksi | ISO 37 |
Kraton® D1163 J (SIS) Linear Block Copolymer Description: Kraton D1163 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |
|||
300% Modulus | 0.000500 GPa | 0.0725 ksi | ASTM D412 |
Dynasol Solprene® 4580X TPE Multiblock Solprene 4580X is a linear multiblock copolymer of styrene and butadiene with high vinyl (>25%), having 45% of styrene content, most of this one appears like block polystyrene, which gives the polym.. |