Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000310 GPa | 0.0450 ksi | ASTM D412 |
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist.. |