Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0400 GPa | 5.80 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0400 GPa | 5.80 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1564 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |