Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0275 GPa | 3.98 ksi | |
Taiwan Sheen Soon Sheenthane® D6050 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0275 GPa | 3.99 ksi | DIN 53504 |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |