Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0219 GPa | 3.18 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |