Polymer Property : 300% Modulus = 0.01700 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.01700 GPa
2.465 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T93 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical prop..