Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01603 GPa | 2.325 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ.. |