Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01500 GPa | 2.176 ksi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |