Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0132 GPa | 1.92 ksi | 150°C, 40 min., Pressure Vulcanization. 24% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25LM Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0132 GPa | 1.92 ksi | |
KKPC KOSYN SOL 5990 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |
|||
300% Modulus | 0.0132 GPa | 1.91 ksi | ASTM D412 |
Styron Buna® SB 1739 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Composition: Buna® SB 1739 – Schkopau is manufactured by cold polymerization using mixed rosin acid /fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE o.. |
|||
300% Modulus | 0.0132 GPa | 1.91 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P Heat Resistant Molding FormulationNordel® IP 4725P |