Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01120 GPa | 1.625 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.01120 GPa | 1.624 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.01120 GPa | 1.625 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.01120 GPa | 1.624 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |