Mechanical Properties Metric English Comments
300% Modulus 0.0112 GPa
1.62 ksi
DIN 53504
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade
IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially..
300% Modulus 0.0112 GPa

@Temperature 145 °C,
Time 2990 sec
1.62 ksi

@Temperature 293 °F,
Time 0.830 hour
cured; ASTM D412
LG Chemical NBR 6230 High Acrylonitrile Polymer
Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m..
300% Modulus 0.0112 GPa
1.62 ksi
DIN 53504
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..