300% Modulus 0.00920 GPa
1.33 ksi
ASTM D412
Styron Buna® cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Composition: Buna® cis 132 – Schkopau is a stereospecific polybutadiene with a high 1,4-cis content. It is manufactured by a solution process using an organo-metallic nickel catalyst which p..
300% Modulus 0.00920 GPa
1.33 ksi
ASTM D412
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00920 GPa
1.33 ksi
Conductive CR Conveyor Belt Cover Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
300% Modulus 0.00920 GPa
1.33 ksi
Compounded, 35 mins.; ISO 37
Dynasol Calprene® 248 Medium CIS Polybutadiene (38%)
Calprene 248 is a medium CIS polybutadiene (38 %), polymerized in solution. This product has an excellent mixing and processing behavior. It is used as ingredient in tire compounds and in other appl..