Mechanical Properties Metric English Comments
300% Modulus 0.008522 GPa
1.236 ksi
ASTM D412
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.008522 GPa
1.236 ksi
ASTM D412
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company