Polymer Property : 300% Modulus = 0.00840 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00840 GPa
1.22 ksi
DIN 53504
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNT..
300% Modulus 0.00840 GPa
1.22 ksi
ASTM D412
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H..