Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.007901 GPa | 1.146 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.007901 GPa | 1.146 ksi | |