Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00785 GPa | 1.14 ksi | |
Taiwan Sheen Soon Sheenthane® A8000F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00785 GPa | 1.14 ksi | |
Taiwan Sheen Soon Sheenthane® A8361E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00785 GPa | 1.14 ksi | |
Taiwan Sheen Soon Sheenthane® AH-585K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmHotmelt adhesive gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00785 GPa | 1.14 ksi | ASTM D412 |
SK Chemicals SKYTHANE® UB420 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |