Mechanical Properties Metric English Comments
300% Modulus 0.00775 - 0.0107 GPa
1.12 - 1.55 ksi
35 min cured; ASTM D412
Iran Petrochemical (PCC) SBR-1712 Styrene Butadiene Rubber
SBR–1712 is staining type cold SBR ,extended with 27.5 part of highly aromatic oil. Provided that the compounds are formulated and processed correctly, the vulcanized SBR–1712 has very g..