Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00740 GPa | 1.07 ksi | |
Taiwan PU Corporation TPU-B85 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00740 GPa | 1.07 ksi | |
Taiwan PU Corporation TPU-BH85 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00740 GPa | 1.07 ksi | |
Taiwan PU Corporation TPUI-L75 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.00740 GPa | 1.07 ksi | DIN 53504 |
Lubrizol ESTANE® T5083 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |