Polymer Property : 300% Modulus = 0.00724 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..