Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 60A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 60A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |