Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00560 GPa | 0.812 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00560 GPa | 0.812 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® G1650 E (SEBS) Linear Block Copolymer Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i.. |
|||
300% Modulus | 0.00560 GPa | 0.812 ksi | Measured on films cast from solution in toluene; ISO 27 |
Kraton® G1650 E (SEBS) Linear Triblock Copolymer Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i.. |
|||
300% Modulus | 0.00560 GPa | 0.812 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |