Polymer Property : 300% Modulus = 0.00470 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00470 GPa
0.682 ksi
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 61 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
300% Modulus 0.00470 GPa
0.682 ksi
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
300% Modulus 0.00470 GPa
0.682 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon..