Polymer Property : 300% Modulus = 0.00379 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00379 GPa
0.549 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.00379 GPa
0.549 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.00379 GPa
0.550 ksi
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3860M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..