Polymer Property : 300% Modulus = 0.00314 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00314 GPa
0.455 ksi
ASTM D3574E
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..