Mechanical Properties Metric English Comments
300% Modulus 0.00270 GPa
0.392 ksi
ASTM D412
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Solprene 4316 is a radial styrene/butadiene block copolymer with 30% styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops propertie..
300% Modulus 0.00270 GPa
0.392 ksi
ASTM D-412
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops proper..