Mechanical Properties Metric English Comments
300% Modulus 0.00241 GPa
0.350 ksi
Kraton® D1116 (SB)n Branched Copolymer
(SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve ..
300% Modulus 0.00241 GPa
0.350 ksi
Machine Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
300% Modulus 0.00241 GPa
0.350 ksi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® G1657 M (SEBS) Linear Block Copolymer
Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id..
300% Modulus 0.00241 GPa
0.350 ksi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G1657 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id..
300% Modulus 0.00241 GPa
0.350 ksi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® D1116 K (SBS) Radial Triblock Copolymer
Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified..
300% Modulus 0.00241 GPa

@Time 7200 sec
0.350 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-9 TPE
Product Description: StarTUFF TF 75-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
300% Modulus 0.00241 GPa
0.350 ksi
ASTM D 412
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Copyright © lookpolymers.com All Rights Reserved