Polymer Property : 300% Modulus = 0.00214 GPa
Polymer Property :
300% Modulus =
0.00214 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
300% Modulus
0.00214
GPa
0.310
ksi
ASTM D412
Network Polymers Softflex® 0470
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.