Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00140 GPa | 0.203 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 172 Styrene - Butadiene Block Copolymer Europrene® SOL T 172 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. The polymer is extended with.. |
|||
300% Modulus | 0.00140 GPa | 0.203 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00140 GPa | 0.203 ksi | Measured on a pressed sample; ISO 37 |
Kraton® D1170 B (SIBS) Linear Triblock Copolymer Description: Kraton D1165 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: .. |