Polymer Property : 300% Modulus = 0.00138 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00138 GPa
0.200 ksi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® D1111 K (SIS) Linear Block Copolymer
Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: ..
300% Modulus 0.00138 GPa
0.200 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1111 K (SIS) Linear Triblock Copolymer
Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: ..
300% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2730 Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2740 Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2835E Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2840E Thermoplastic Elastomer
Information provided by Teknor Apex Company