300% Modulus 0.00108 GPa

@Time 7200 sec
0.156 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE
Product Description: StarFlex P 7350-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem 475-860N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem 8075 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem AB760LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.00108 GPa
0.156 ksi
JIS K6301
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..