Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000700 GPa | 0.102 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 9131 Styrene - Isoprene Block Copolymer Europrene® SOL T 9131 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 15% weight and diblock content is.. |