Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000345 GPa | 0.0500 ksi | Typical properties of film cast form toluene solution; ASTM D412 |
Kraton® D1113 P (SIS) Linear Block Copolymer Description: Kraton D1113 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra.. |
|||
300% Modulus | 0.000345 GPa @Time 7200 sec |
0.0500 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7025-1000 TPE Product Description: StarMediflex P 7025-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
300% Modulus | 0.000345 GPa | 0.0500 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 1900 Thermoplastic Elastomer Information provided by Teknor Apex Company |