Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 58.6 - 86.2 MPa @Thickness 0.508 mm |
8500 - 12500 psi @Thickness 0.0200 in |
1018 steel; ASTM C633-01 |
The NanoSteel® Company SHS 7570 TWAS Steel Alloy, Cored Wire Coating Description: SHS 7570 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional combined wear, impact and corrosion resistance in high chlorine, salt fog, c.. |