Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 6.55 MPa @Temperature 82.2 °C |
950 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-34 Epoxy Adhesive This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste.. |