Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.410 MPa
59.5 psi
Typical lap shear
Momentive Performance Materials RTV157 Gray Adhesive Sealant, High Strength Paste
One-part cure. Typical uses: High strength adhesive; use for gasketing, aircraft maintenance, and electrical insulation.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of..
Adhesive Bond Strength 0.410 MPa
59.5 psi
Typical lap shear
Momentive Performance Materials RTV159 Red Adhesive Sealant, High Strength Paste
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance..