Polymer Property : Adhesive Bond Strength = 5700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.621 - 39.3 MPa
90.0 - 5700 psi
Average value: 8.98 MPa Grade Count:51
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..