Polymer Property : Adhesive Bond Strength = 540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.72 MPa
540 psi
Chloroprene-Chloroprene; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 3.72 MPa
540 psi
Natural Rubber-Natural Rubber; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..