Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 5.03 MPa | 730 psi | Lap shear, alum to alum, 15 min @ 100°C |
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior .. |
|||
Adhesive Bond Strength | 5.03 MPa | 730 psi | to Oriented Polypropylene (OPP) @ 600°F, 1.0 mil coating onto 50 lb Kraft paper; Dow Method |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |
|||
Adhesive Bond Strength | 5.03 MPa | 730 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond 516H01 Low Viscosity Room Temperature Cure Adhesive TRA-BOND 516H01 is a room temperature curing, low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors, including Pre-Mixed and Frozen applications. It has also been use.. |