Polymer Property : Adhesive Bond Strength = 4950 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 34.1 MPa
4950 psi
Steel-Steel; after optimum cure
Armstrong A-706 Epoxy Adhesive
A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m..