Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 49.0 MPa | 7100 psi | Steel-Steel; after optimum cure |
Armstrong A-40 Epoxy Adhesive Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re.. |