Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 32.3 MPa @Thickness 1.60 mm |
4690 psi @Thickness 0.0630 in |
CRS plate |
Dow BETAMATE™ 73345G Epoxy BETAMATE™ 73345G is a one-part, high performance, heat curing, epoxy adhesive. It is capable of bonding oily galvanized and cold rolled steel without a primer and has corrosion resistance. BETAMA.. |