Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 32.0 MPa | 4640 psi | steel collar and pin shear; ISO 10123 |
Permabond HH167 Anaerobic Retainer Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli.. |